It will be easier to sand and will bond to the styrene better just rough up the styrene before you apply it to help promote adhesion. The squadron will shrink over time and you will not be happy. This stuff is a two part filler and it will make the body work more enjoyable to do.
__________________
AKA "00" Biddle RIP FreddyGearDrive 2-12-59/12-19-11 |
#22
|
|||
|
|||
![]()
the glaze coat flows so much better than just bondo , it fills in little pin holes better, and it is easier to sand. when i worked at a body shop that is what we would use as the final coat of filler before we would primer a car.
|
#23
|
||||
|
||||
![]()
Decided to start over, body work is not for me. Going with more of a stock King Hauler look. Need a new body!
|
![]() |